Abstract

CERROBEND Alloy is a bismuth-base eutectic alloy that melts at 158 F (70 C). It is low melting temperature and controlled-shrinkage characteristics make it highly useful industry for such applications as anchoring bushings in drill jigs, cores for spinning and tube-bending filler. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on casting, forming, heat treating, and machining. Filing Code: Bi-6. Producer or source: Cerro Metal Products.