Abstract

Kaiser Alloy 1100 is in the commercially pure wrought family (1000 or 1xxx series) of aluminum alloys. It is typically used in applications requiring maximum ductility and relatively low strength. It has good corrosion resistance, workability, and weldability. This datasheet provides information on composition, physical properties, hardness, elasticity, and shear strength as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as machining and joining. Filing Code: Al-459. Producer or source: Kaiser Aluminum Corporation.