Abstract

This producer has pioneered the development of the -T77 temper, a high strength corrosion resistant temper for Alloy 7150 plate and extrusions. Alloy 7150-T77 provides weight savings opportunities in structure governed by static strength requirements but where "overaged" condition corrosion resistance is required. This datasheet provides information on composition, tensile properties, and compressive strength. It also includes information on corrosion resistance as well as forming. Filing Code: Al-442. Producer or source: Alcoa Mill Products Inc..