Abstract

Kaiser Alloy 7003 is a medium strength alloy originally developed in Japan. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as forming and joining. Filing Code: AL-434. Producer or source: Kaiser Aluminum.