Abstract

Alcoa alloy 6013 Power Plate is a higher machinable development with higher strength over 6061-T651 by 22%. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: AL-425. Producer or source: Alcoa.