Alcan 5086 is used in the aerospace industry, particularly when good mechanical properties and outstanding corrosion resistance are required. This datasheet covers Alcan 5086 alloy in O and several H tempers as tubing. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on forming, machining, and joining. Filing Code: AL-420. Producer or source: Alcan Inc.