Abstract

Finkl Alu-X is a modification of UNS A92618 with higher thermal conductivity than many aluminum alloys used for molds. The alloy, when forged, solution treated, and stabilized, is well suited for pressure applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on casting, machining, joining, and surface treatment. Filing Code: AL-363. Producer or source: A. Finkl & Sons Company.