Abstract

The Al-2wt.%Cu matrix composite contains 60 vol.% alumina. The aluminum ceramic fiber is Nextel 610, which affects the longitudinal direction, resulting in a high longitudinal specific modulus and a specific strength with good off-axis properties. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information on corrosion resistance. Filing Code: AL-345. Producer or source: 3M.