Lanxide 91-X-1060-30P is a metal-matrix composite (MMC) consisting of an aluminum-silicon magnesium alloy matrix and 30 vol.% of silicon carbide. The MMC is designed to outperform its unreinforced counterpart. It is available as sand castings with a T6 heat treatment. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as fracture toughness and fatigue. It also includes information on forming. Filing Code: AL-342. Producer or source: Lanxide Corporation.