UltrAlloy is a lead-free, enhanced machining product with the inherent benefits of a 6xxx-series alloy. The alloy is produced as a cold-finished rod and bar with strength levels comparable to 6262. The alloy is registered with the Aluminum Association as X6020. This datasheet provides information on composition, microstructure, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, machining, joining, and surface treatment. Filing Code: AL-340. Producer or source: ALCOA Wire, Rod & Bar Division. Originally published September 1996, corrected December 1996.