Abstract

Lanxide 93-X-3027 is an aluminum magnesium alloy with 50 or 60 vol.% of aluminum oxide. This metal-matrix composite is designed to outperform the unreinforced counterpart. This datasheet provides information on composition, physical properties, microstructure, elasticity, and tensile properties as well as fracture toughness and creep. Filing Code: AL-339. Producer or source: Lanxide Corporation.