Abstract
ALUMINUM ALLOY 201.0 is a structural casting alloy available as sand, permanent mold and investment castings. It is used in structural casting members, applications requiring high tensile and yield strengths with moderate elongation, and where high strength and energy-absorption capacity are needed. This datasheet provides information on composition, physical properties, and elasticity as well as creep and fatigue. It also includes information on high temperature performance as well as casting, heat treating, machining, joining, and surface treatment. Filing Code: AL-336. Producer or source: Various aluminum companies.