Abstract

ALUMINUM ALLOY(S) 206.0 and A206.0 are structural castings in the heat treated temper for applications requiring high tensile and yield strengths with moderate elongation. This datasheet provides information on composition, physical properties, tensile properties, and compressive, shear, and bearing strength as well as fatigue. It also includes information on as well as heat treating. Filing Code: AL-335. Producer or source: Various aluminum companies.