Abstract

AA 3105 is a non-heat treatable aluminum alloy with excellent weldability, formability and corrosion resistance. It is used in residential siding and rain carrying goods. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-289. Producer or source: Various aluminum companies.

This content is only available as a PDF.