FEDERATED F024 is an aluminum sand casting alloy characterized by moderate strength, good pressure tightness and excellent resistance to corrosion and staining. Its uses include such items as marine hardware and cooking utensils. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength. It also includes information on corrosion resistance as well as casting, heat treating, and machining. Filing Code: Al-227. Producer or source: Federated Metals Corporation, ASARCO Inc..