Abstract

Aluminum X7005 is an age-hardenable aluminum alloy having high mechanical properties, good fracture toughness, good corrosion and stress-corrosion resistance, and good weldability. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-151. Producer or source: Aluminum Company of America.