SAP is a special Sintered Aluminum Powder characterized by high tensile strength at room temperature and at elevated temperatures. It features a range of useful engineering properties. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, machining, joining, and powder metal forms. Filing Code: Al-146. Producer or source: Aluminium Industrie Atkiengesellschaft.