Abstract

Alcan 432 is a natural aging aluminum sand casting alloy that is not susceptible to stress corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-136. Producer or source: Aluminum Company of Canada Ltd.