Abstract

Aluminum C355 is a high purity permanent mold casting alloy that responds to an age-hardening heat treatment. It has superior properties to those of standard Aluminum 355. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on casting, heat treating, machining, and joining. Filing Code: Al-115. Producer or source: Aluminum Company of America.