Abstract

TENS-50 is a high strength aluminum casting alloy that responds to an age-hardening heat treatment. This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive, shear, and and bearing strength It also includes information on high temperature performance as well as casting, heat treating, machining, and joining. Filing Code: Al-92. Producer or source: Navan Products Inc..