Abstract

ALUMINUM 357 is a highly purity aluminum casting alloy which develops high tensile and yield strengths with good ductility after heat treatment. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-80. Producer or source: Kaiser Aluminum & Chemical Corporation.