Abstract

NORAL 62S is an aluminum extrusion alloy that responds to an age hardening heat treatment. It has good strength and excellent fabricating characteristics. This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive, shear, and bearing strength as well as fracture toughness and fatigue. It also includes information on as well as forming, heat treating, machining, and joining. Filing Code: Al-77. Producer or source: Northern Aluminium Company Ltd.