Aluminum 2618 is a heat treatable aluminum alloy recommended for high temperature applications up to 575 F. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as creep and fatigue. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: Al-76. Producer or source: Kaiser Aluminum & Chemical Corporation.