KYNAL P5 is a grade of pure aluminum having high corrosion resistance, electrical and thermal conductivity. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-49. Producer or source: Imperial Metal Industries Ltd.