ALCAN 26S is a wrought heat treatable aluminum alloy recommended for structural applications requiring high strength. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-41. Producer or source: Aluminum Company of Canada Ltd.