ALUMINUM 7001 is a heat treatable, high strength, structural aluminum alloy. It was formerly known as ALUMINUM HZM-100. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-22. Producer or source: Harvey Aluminum Company. Originally published January 1955, revised January 1963.