CIMET is a low nickel, high chromium-iron alloy suitable for sulfur-bearing fuel applications. It is resistant to heat, corrosion, and abrasion. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: SS-107. Producer or source: Driver-Harris Company.