Abstract

KETOS is an oil-hardening non-deforming tool steel having deep hardening qualities with a fine grain structure. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as deformation. It also includes information on forming, heat treating, and machining. Filing Code: TS-96. Producer or source: Crucible Steel Company of America.