Abstract
VASCO CHOICE No. 1 is a 4% chromium high-carbon hot work steel especially adapted for those operations where the hot work is performed by a compressive action. This datasheet provides information on composition, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, and machining. Filing Code: TS-95. Producer or source: Vanadium Alloys Steel Corporation.