UNITEMP 212 is a precipitation hardening steel that will maintain high strength and corrosion resistance up to 1400 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as heat treating, machining, joining, and surface treatment. Filing Code: SS-105. Producer or source: Cyclops Corporation.