Abstract

USS STRUX is an alloy steel designed for use in the heat treated condition at a minimum tensile strength of 280,000 psi. At this very high strength level the steel has adequate ductility and notch toughness for critical applications. This datasheet provides information on composition and tensile properties. Filing Code: SA-100. Producer or source: United States Steel Corporation.