Abstract

Ti-4A1-3Mo-IV is an alpha-beta type titanium alloy having a good combination of high strength, creep and stability at elevated temperatures. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear, bearing, and bend strength as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ti-26. Producer or source: Titanium Metals Corporation of America.

This content is only available as a PDF.