Abstract

REVERE No. 469 is an arsenical bronze that can be readily extruded and forged. It has good machinability, wear and corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-87. Producer or source: Revere Copper and Brass Inc..