Abstract

ELECTRITE COBALT is a 5% cobalt type high-speed steel recommended for heavy duty cutting tools. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-89. Producer or source: Latrobe Steel Company.