Abstract

TIMKEN DM is a low carbon, chromium-molybdenum alloy steel recommended for high temperature applications up to 1200 F. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as fracture toughness and creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-95. Producer or source: Timken Roller Bearing Company.