Abstract

UNITEMP-14MV is a silicon-chromium-molybdenum-vanadium alloy steel having high resistance to thermal cracking and heat checking, even in a highly hardened condition, and also has good shock resistance at high hardness levels. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: SA-106. Producer or source: Cyclops Corporation.