INCONEL 700 is an age-hardenable heat and corrosion resisting nickel-base alloy. It has high stress-rupture characteristics. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-33. Producer or source: International Nickel Company Inc.. Originally published April 1957, revised November 1960.