Abstract
Magnesium ZE41A is a magnesium-base casting alloy containing zinc, zirconium and rare earths. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear andbearing strength as well as creep and fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Mg-48. Producer or source: The Dow Metal Products Company.
This content is only available as a PDF.
Copyright © ASM International® 1996
1996
ASM International
Topics
Corrosion-resistant alloys
High-temperature alloys
Cast magnesium alloys
Magnesium alloys
Chemical composition
Castability
Heat treatability
Joinability
Machinability
Creep properties
Elastic modulus
Fatigue properties
Hardness
Shear strength
Tensile properties
Physical properties
Thermal properties