Abstract
Ti-13V-11Cr-3Al is a high strength, meta-stable beta titanium-base alloy recommended for service in the temperature range of -65 to plus 600 F. It responds to an age-hardening heat treatment. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ti-27. Producer or source: Titanium Metals Corporation of America.