Abstract

STAMINAL is a shock resisting steel having high toughness and fair wear resistance. It can be air or oil hardened. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-98. Producer or source: Latrobe Steel Corporation.