Type CE-30 is a 29% Cr-9% Ni corrosion resisting casting alloy. It has high degree of stability against intergranular corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: SS-108. Producer or source: Stainless steel foundries.