Abstract

Amsco Manganese Steel is a high-carbon high-manganese austenitic steel recommended for wear and abrasion resisting applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on casting, forming, heat treating, machining, and joining. Filing Code: SA-105. Producer or source: American Manganese Steel Division.