Abstract

COLHED is a carbon-vanadium tool steel made especially for cold heading dies. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, and machining. Filing Code: TS-83. Producer or source: Vanadium Alloys Steel Company.