BERYLCO 50 is a beryllium copper alloy offering high electrical conductivity and resistance to wear. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating, machining, joining, and surface treatment. Filing Code: Cu-78. Producer or source: Beryllium Corporation.