Abstract
FERRO-TIC C is a machinable grade of cemented carbide which can be hardened by oil quenching. This datasheet provides information on composition, physical properties, hardness, elasticity, and compressive strength as well as creep. It also includes information on forming, heat treating, and joining. Filing Code: TS-82. Producer or source: Sintercast Corporation of America.