Abstract

PEARLITIC MALLEABLE IRON is a high strength cast iron recommended for dependable service, strength and machinability in highly stressed parts at work in mobile and stationary mechanisms. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: CI-26. Producer or source: Albian Malleable Iron Company.