LEADED NAVAL BRASS is a free-cutting copper-zinc alloy having high strength, toughness and corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-84. Producer or source: Brass mills.