Abstract
KYNAI C69 is an age-hardenable aluminum alloy recommended for medium and high strength appIications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Al-87. Producer or source: Imperial Chemical Industries Inc..