Abstract

CARPENTER No. 883 is a 5% chromium hot work steel designed particularly for applications requiring extreme toughness combined with good red-hardness. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness and creep. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-86. Producer or source: Carpenter.