MicroMack is a nitrogen-containing austenitic stainless steel similar to Type 301 stainless but having higher ductility in the full hard condition. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-96. Producer or source: Washington Steel Corporation.